Variety | Holocellulose density μg·mm−3 | Lignin density μg·mm−3 | Cellulose density μg·mm− 3 | Hemicellulose density μg·mm− 3 |
---|---|---|---|---|
2015 | ||||
 Takanari | 147.6 | 32.4 | 92.3 | 55.2 |
 Koshihikari | 107.7 | 26.1 | 66.2 | 41.4 |
 | * | ** | * | ns |
2016 | ||||
 Takanari | 165.2 | 24.8 | 104.3 | 60.9 |
 Koshihikari | 123.3 | 9.8 | 85.8 | 37.6 |
 | * | ** | * | * |